NILIT Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardency. The halogenated flame retardant system used in this product allows a wide range of colors. This product does not contain the flame retardants mentioned in the WEEE directive (PBB or PBDE). The product is used widely throughout the electrical and appliance industries for applications like pressure switches, circuit breaker housings, contactors, timers and programmers.Key characteristics: - UL listed V0 at 3.0 and 0.75 mm
- UL listed GWIT 825 °C and GWFI 960°C at 0.75 mm, compliant with IEC 60335-4
- UL listed on CTI PCL 1 (CTI = 425 V)
- Excellent mechanical performance
- Colorable in light colors
- Easy processing
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Zone 4
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Clamping Force
- Flammability Rating
- Heat Resistance - Ball Test
- Holding Pressure
- Needle Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|