NILIT Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price/performance ratio and can be colored in almost any color. It does not cause any corrosion of or deposits on electrical contacts. Lasermarking grades with a very good contrast are available.Key characteristics: - UL 94 V2 at 0.75 mm
- Halogen and red phosphorous free
- Good overall mechanical performance
- Low density
- Colorable in a wide range of colors
- Easy processing, fast cycling
- No corrosion of or deposits on electrical contacts
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Heat Resistance - Ball Test
- Needle Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|