NILIT Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT
Subcategory: Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes: Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used for applications that need a high dimensional stability, like automotive connectors, transmission housings for electro motors or parts that are subjected to high UV radiation, like exterior automotive parts.Key characteristics: - Good overall mechanical performance
- Low moisture absorption
- Good UV resistance
- Good thermal performance
Information provided by NILIT.
| Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
- Heat Resistance - Ball Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|