Sam Yang Kasei Trirex® Grade PC-3020HF 22 MFI Clear Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Key Words: Polymer Technology & Services, LLC (PTS)
Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Transmission, Visible
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
- Clamp Pressure
- Cycle Time - Injection
- Cycle Time - Cooling
- Vent Depth
- Screw Speed
- Injection Speed- Edge Gate
- Injection Speed- Tab Gate
- Injection Speed- Tunnel Gate
- Shot Size
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|