Chi Mei Polylac® PA707 ABS Resin - General Purpose
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: Information provided by US distributor Calsak Corporation.
Key Words: Poly(Acrylonitrile Butadiene Styrene); Calsak Corporation
Material Notes: High gloss, High rigidity, Medium Flow Typical properties; not to be construed as specifications. Mechanical properties measured on 1/8 in. Type I specimens.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|