Chi Mei ACRYSTEX® PM-600 Methyl Methacrylate Styrene
Subcategory: Polystyrene; Acrylic; Thermoplastic
Key Words: Calsak
Material Notes: Product Characteristics- Residuals, Low
- Water Absorption, Low to none
- RoHS Compliant
- Weather Resistance, Good
Applications - Appliances
- Household Goods
- Building Materials
- Optical Applications
- Containers, Food
- Toys
Information provided by Calsak Corporation
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |