Chi Mei KIBITON® PB-5925 Q Resin, General Purpose
Subcategory: Styrene-Butadiene; Thermoplastic
Key Words: Calsak
Material Notes: Information provided by Calsak Corporation
| Available Properties |
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Vicat Softening Point
- Haze
|
|
|
|