CCC Chemicals EL-PRO™ P841J Polypropylene Clarified Copolymer
Subcategory: Polypropylene; Thermoplastic
Key Words: Calsak
Material Notes: Product Characteristics- High flowability
- High stiffness
- Good clarity
- High impact strength
Applications - Electrical appliance parts
- Washing machine parts, base, tub, control panel
Information provided by Calsak Corporation
| Available Properties |
- Specific Gravity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|