CCC Chemicals EL-LENE™ H5818J HDPE Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: Calsak
Material Notes: Product Characteristics- Good Processability
- Good stiffness good impact strength balance properties
- Odorless
- Food Contact
Applications - General purpose injection parts such as housewares
- Office articles, toy parts, bottle caps
Information provided by Calsak Corporation
| Available Properties |
- Specific Gravity
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Vicat Softening Point
|
|
|
|