CCC Chemicals EL-LENE™ H5840B HDPE Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: Calsak
Material Notes: Product Characteristics- Excellent environmental stress cracking resistance
- Good appearance, odorless, food contact
- Good printability
Applications - Bottles for food, juice, soft drinks, milk, detergent, cosmetics, medical products, lube oil, brake fluid, chemicals, etc.
Information provided by Calsak Corporation
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|