Plenco 02567 Single-Stage Phenolic, Granular, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under component file E40654. 02567 is available in black, brown, or red color. 02567 Black is not intended for electrical insulating applications. Information supplied by Plenco.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact, Notched
- Impact
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|