Plenco 04504 Two-Stage Phenolic, Granular, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical properties, it has found use in a wide variety of wiring device applications. It is UL recognized under file E40654. Information supplied by Plenco.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact, Notched
- Impact
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|