Plenco 05118-T5 Two-Stage Phenolic, Granular, Injection Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, very low water absorption, and good dimensional stability under severe exposure. 05118 is available in grey. Information supplied by Plenco.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact, Notched
- Impact
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|