Plenco 05482 Two-Stage Phenolic, Granular, Transfer Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for electrical insulating applications. Information supplied by Plenco.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact, Notched
- Impact
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Oxygen Index
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|