Plenco 07300 Organic and Fiber Filled Novolac Phenolic, Nodular, Injection Molded
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: This is no longer a part of the Plenco standard product line.
Material Notes: Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file E40654. 07300 is available in black. Information supplied by Plenco
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Charpy Impact, Notched
- Impact
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|