Lendell Manufacturing Nolatex®
Subcategory: Polyurethane, TS; Thermoset
Material Notes: Latex FreeThis form is used in the cosmetic industry. Nolatex ® also possesses insulation qualities. Applications: Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Makeup Pads, Cosmetic Pads in Advertising Mailouts, Nail Shiners, Makeup Remover Pads, Gasket Material for Toner Cartridges, and Battery Insulator Wraps Information provided by Lendell Manufacturing Inc.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Compression Set
- % Volume Swell
- CLD 50%
- CLD 50% R
- Comfort Factor
- Expansion, %
- Hysteresis
- IFD 25% R
- IFD 25% RRT
- IFD 65%
- Recovery
- Sag Factor
- Water Retention, %
- Wet Out, minutes
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|