Lendell Manufacturing Supersoft Foams
Subcategory: Polyurethane, TS; Thermoset
Material Notes: Angel SkinThis line of foam has excellent feel and touch characteristics, as well as absorbency. The "breath-ability" of these foams, due to their high moisture vapor transmission qualities and the soft feel makes them ideal for skin contact applications. The foam is also formulated for use in the medical field. Applications: Outdoor Apparel, Boots, Gloves, Skin Contact Applications, Bed Comforters, Ski Goggles Lense Cleaner, Foam with Metal Dust, "New Grit" Abrasive Foam Blocks, Mattresses and Pillows Information provided by Lendell Manufacturing Inc.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Yield
- Tear Strength
- Compression Set
- CLD 50%
- CLD 50% R
- Comfort Factor
- Expansion, %
- Hysteresis
- IFD 25% R
- IFD 25% RRT
- IFD 65%
- Recovery
- Sag Factor
- Water Retention, %
- Wet Out, minutes
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|