Plenco VALITE 4100 Novolac Phenolic, Granular, Injection Molded
Subcategory: Phenolic; Thermoset
Close Analogs: Plenco has discontinued their Valite product line.
Material Notes: This Valite product has been replaced by Plenco 4100. Data provided by Plenco. VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in applicance and oil field applications and can be molded by compression, transfer, or injection processes. It is UL recognized under component file E59891. VALITE 4100 is the same formulation as PLENCO 04100. Plenco drop ball 113g test value is 26 cm.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Charpy Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|