Plenco VALITE 4224 Novolac Phenolic, Granular, Transfer Molded
Subcategory: Phenolic; Thermoset
Close Analogs: Plenco has discontinued their Valite product line.
Material Notes: This Valite product has been replaced by Plenco 4224. Data provided by Plenco. VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive applications and can be molded by compression, transfer, or injection processes. Plenco drop ball 113g test value is 35 cm.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Charpy Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|