Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.
Material Notes: Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particularly suited for mechanical parts with thin sections that require wheelabrating, staking or pulling of inserts.Data provided by Plaslok Corporation.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|