Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.
Material Notes: Plaslok 302 is a two-stage, woodflour and flock-filled phenolic molding compound. It has low specific gravity, broad molding latitude and an excellent balance of electrical and physical properties. Its high impact strength makes it particularly well suited for thin wall parts, or where mechanical stress is experienced during assembly.Data provided by Plaslok Corporation.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|