Plaslok PlasGlas™ 50112 Heat Resistant Glass Filled Thermoset Polyester BMC
Subcategory: Polyester, TS; Thermoset; Polymer
Close Analogs: Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.
Key Words: Bulk Molding Compound
Material Notes: PlasGlas 50112 is a glass-filled polyester bulk molding that has been specially formulated to have the good heat-resistance, dimensional stability, and smooth surface required to function well as automotive halogen headlamp reflectors. It can be compression, transfer, or injection molded and is available in either bulk or extruded form.Data provided by Plaslok Corporation.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|