LG Chemical LUPOL GP-3402 General Purpose Polypropylene, 40% Mineral Fillers, High Modulus, High Flow
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics. Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner, mud guard, door trim, garnish Electrical and Electronic: Tail lamp housing, air conditioner housing, fan, socket, washing machine parts Industrial Parts and Household Appliance:Propeller fan, pulley, container, pump container, pump casing, handle and switch cover of electric jar, fan shroud/support
Information Provided by LG Chem
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|