LG Chemical KEYFLEX BT-1047D Thermoplastic Ester for Injection Molding, 47D Hardness
Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic
Material Notes: KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber and the strength of engineering plastics. In additions, they offer very good thermal stability, chemical resistance and weather resistance. KEYFLEX resins can be widely accepted as the replacement of thermoset rubbers. Characterization: - High impact strength
- Low specific gravity
- Excellent resistance to chemicals and weathering
- Good electrical properties
- Various hardness grades (soft, semi-soft, and hard)
- Colorability
- Recyclability
Applications: Automotive: Bumper, timer ELR parts, safety belt hook, packing parts, actuator, fuel tank, remote control button Cable: Cable insulation, high pressure hose, wire clamp, telephone wire, computer cord, nut seal, seal parts Electrical and Electronic: Connector cover, connector, rubber switch, spring, timing belt Others: Film and sheet, packingless cap, hose, flexible coupling packing, conveyor belt, sealing parts.
Information Provided by LG Chem
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tear Strength
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|