LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
Subcategory: Thermoplastic
Material Notes: LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solving problems associated with build-up of electrostatic charges, electrostatic discharge, and electromagnetic interference. These materials span the surface resistivity spectrum from antistatic through conductive to EMI shielding (100-1012O). Applications: I.C. tray, wafer carrier, I.C. magazine, notebook PC case, home appliance part, LCD cassette tray Information Provided by LG Chem
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|