LG Chemical TR-556 Transparent ABS for Extrusion, Natural and Colored Pellets
Subcategory: ABS Polymer; Thermoplastic
Material Notes: LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electronic parts, OA machines, toys and others that require transparency and high impact strength. An Izod impact strength or falling dart impact strength of LG transparent ABS is relatively similar to that of general ABS, it is not easily cracked like SAN or PMMA resin in the condition of low impact energy. TR-556 is specially designed for sheets such as sound proofing walls and canopy applications. Since LG transparent ABS TR-556 has excellent transparency and property balance, it could easily be applied on the following products: Electric and electronic: Vacuum cleaner parts, air-conditioner panel, humidifier water tank, mixer housing, copier parts, telephone parts, computer housing, facsimile parts, printer panel, washing machine panel and cover, electric fan stand, TV front frame, windows of microwave ovens, calculators, semiconductor carrier boxOther Applications: Compact cases, cosmetic parts, tool handles, toys, stationeries, game machine Information Provided by LG Chem
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Flammability, UL94
- Haze
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Adapter Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Roll Temperature
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|