LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
Subcategory: ABS Polymer; Thermoplastic
Material Notes: LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electronic parts, OA machines, toys and others that require transparency and high impact strength. An Izod impact strength or falling dart impact strength of LG transparent ABS is relatively similar to that of general ABS, it is not easily cracked like SAN or PMMA resin in the condition of low impact energy. TR-558 series is good for applications requiring high stiffness.Information Provided by LG Chem
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Index of Compound
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Flammability, UL94
- Haze
- Transmission, Visible
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Adapter Temperature
- Die Temperature
- Melt Temperature
- Mold Temperature
- Roll Temperature
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|