LNP Thermocomp® PF-1006 HS MC-1 BK8-115 Nylon 6, 30% Glass Fiber
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Glass Fiber Fortified, Heat Stabilized. Typical properties below provided by LNP Engineering Plastics.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Unnotched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|