LNP (SABIC Innovative Plastics) LEXAN® LCF1515 Polycarbonate, 15% Carbon Fiber Reinforced, PTFE Lubricant
Subcategory: Polycarbonate; Thermoplastic; Polymer
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
- Features: Lubricated, High Strength, Good Abrasion Resistance, Good Dimensional Stability
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Clamp Pressure
- Shot Size
- Vent Depth
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|