LNP (SABIC Innovative Plastics) NORYL® HM3525 Polyphenylene Ether + Polystyrene
Subcategory: Polystyrene; Polyphenylene Ether/PPO; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Specific Gravity
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |