LNP (SABIC Innovative Plastics) NORYL® MX5817 Polyphenylene Ether + Polystyrene, 19.5% Glass / Carbon Fiber Reinforcement
Subcategory: Polystyrene; Polyphenylene Ether/PPO; Thermoplastic; Polymer
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Electrical Applications - Features: Low Warpage
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Specific Gravity
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Shot Size
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|