LNP (SABIC Innovative Plastics) Stat-Kon® LCL-4026 EM BK8-115 Polyetheretherketone, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant by weight
Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic; Polymer
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes:
- Features: Electrically Conductive, Good Moldability, Lubricated
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Tensile Strength at Break
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|