LNP (SABIC Innovative Plastics) NORYL® PX5379 Polyphenylene Ether + Polystyrene, 10% Glass Fiber Reinforcement
Subcategory: Polystyrene; Polyphenylene Ether/PPO; Thermoplastic; Polymer
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Typical applications are TV chassis, deflection yokes and connectors. - Features: Flame Retardant, Low to None Halogen Content
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Hardness, Rockwell L
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Back Pressure
- Shot Size
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text