LNP (SABIC Innovative Plastics) ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant
Subcategory: Polyetherimide; Thermoplastic; Polymer
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500. - Features: Lubricated, Good Wear Resistance
- Forms: Pellets
Information provided by LNP, a GE Plastics Company.
| Available Properties |
- Specific Gravity
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Falling Dart Impact
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|