Loctite® U-05FL Metal bonder, highly flexible, high peel, high shear Durabond® Urethane Adhesive
Subcategory: Adhesive; Polyurethane, TS; Thermoset
Material Notes:
Urethane Adhesives Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.
Loctite® U-05FL Metal bonder, highly flexible, high peel, high shear Durabond® Urethane Adhesive A two-part, high-performance urethane adhesive for metal bonding with a 5-minute worklife. Off-white, highly flexible, impact resistant, high peel, high sheer.
- Mix Ratio by Volume, Resin:Hardener = 1:2
Bonding Type: Urethane
| Available Properties |
- Viscosity
- Hardness, Shore D
- Shear Strength
- Peel Strength
- Dielectric Strength
- Glass Temperature
- Pot Life
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|