Loctite® 3105 Acrylic Light Cure Adhesive
Subcategory: Adhesive; Acrylic; Thermoset
Material Notes:
Acrylic Light Cure Adhesives Versatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single component, solvent-free products cure in seconds when exposed to UV/visible light sources. Some light cure adhesives can be combined with activator curing methods to meet specific application requirements.
Loctite® 3105 Acrylic Light Cure Adhesive A high strength, low viscosity, UV/visible light cure adhesive. Primarily designed for bonding rigid and flexible PVC to polycarbonate. Enables easy assembly of components with close fitting tolerances. Recommended for applications involving small gaps less than 0.25 mm. Key Substrates: Polycarbonate, thermoplastic, polyvinylchloride Cure Type: Ultraviolet, visible
| Available Properties |
- Brookfield Viscosity
- Hardness, Shore D
- Elongation at Break
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|