Loctite® 272 High Temperature/High Strength Threadlocker
Subcategory: Adhesive; Thermoset
Material Notes:
Threadlockers Invented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from delicate electronic components to heavy construction equipment. Loctite® Pre-Applied Threadlockers are dry-to-the-touch films applied to threaded fasteners by fastener suppliers and process centers located throughout North America. Ideally suited for OEMs, they improve speed of assembly and ensure quality by eliminating on-line adhesive dispensing. Loctite® Threadlockers are available in varying viscosities and strengths for virtually any application, including exposure to extreme environments.
Loctite® 272 High Temperature/High Strength Threadlocker Withstands temperatures to 450ºF. Provides a fast cure on most surfaces including "as received" fasteners. Recommended for bolts up to 1.5" (36 mm) in diameter. Heat and hand tools are required for disassembly. Torque capability, M10 steel nuts and bolts: 200 in. lbs. (break), 220 in. lbs. (prevail). Recommended Primer: 7649(N) or 7471(T) Typical Use: High temperature applications
| Available Properties |
- Density
- Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|