Loctite® 660 Press Fit Repair Quick Metal® Retaining Compound
Subcategory: Adhesive; Thermoset
Material Notes:
Retainers Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. Finding wide acceptance as a standard method for assembling press and slip-fitted parts, Loctite® Retaining Compounds fill the "inner space" between components and cure to form a strong precision assembly. Formulated in a selection of viscosities, gap filling ability, flexibility and strength characteristics, Loctite® Retaining Compounds can be applied with automatic process equipment or dispensed manually.
Loctite® 660 Press Fit Repair Quick Metal® Retaining Compound A creamy, non-running adhesive/sealant. Repairs worn machine parts. Restores correct fit to mating assemblies. Fills gaps up to 0.020" diameter clearance. Recommended Primer: 7649 (N). Agriculture Canada approved Typical Use: For repair of worn machinery parts
| Available Properties |
- Density
- Viscosity
- Shear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Color
- Gap Fill
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|