Loctite® 5206 Flexible Cure Flange Sealant
Subcategory: Adhesive; Thermoset
Material Notes:
Anaerobic GasketingLoctite® 5206 Flexible Cure Flange Sealant Slow curing allows for micro-movement during assembly operations. Good sealing properties against oil and water/glycol. High viscosity. Recommended Primer: 7649 (N) or 7471 (T). Typical Use: Slow curing, flexible
| Available Properties |
- Density
- Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Cure Time
- Color
- Gap Fill
|
|
|
|
| Property Data |