Loctite® 384 1 component acrylic Output™ Thermally Conductive Repairable Acrylic Adhesive
Subcategory: Adhesive; Acrylic; Thermoset
Material Notes:
Acrylic Bonding Adhesives and Thermally Conductive Bonders Loctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond. Loctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or microprocessors and their heat sinks. Loctite offers a wide range of adhesive chemistries including silicones, acrylics and epoxies. Many processing options are available for curing these adhesives such as heat cure, activator cure, and UV light.
Loctite® 384 1 component acrylic Output™ Thermally Conductive Repairable Acrylic Adhesive Mounts components to heat sinks but allows removal for repair or replacement. Output™ Activator is required for curing. A repairable, room temperature curing adhesive used for parts subject to disassembly. Recommended Primer: Output™ Activator 20263. Cure Type: Activator 7387 Bonding Type: Acrylic Typical Use: Repairable adhesive for parts subject to disassembly
| Available Properties |
- Density
- Viscosity
- Tensile Modulus
- Shear Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
- Cure Time
- Cure Time
- Shelf Life
- Color
- Gap Fill
- Viscosity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|