Loctite® 394 Acrylic/urethane UV Shadowcure™ Coating
Subcategory: Adhesive; Acrylic; Thermoset
Material Notes:
Conformal Coatings Conformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.
Loctite® 394 Acrylic/urethane UV Shadowcure™ Coating For high reliability applications where superior moisture and mechanical abrasion resistance are required. No solvents. Low VOC. Cure Type: UV or Catalytic MIL-I-46058C Approved; UL-746C Approved; IPC-CC-830A Approved; Bellcore TR-NWT-000078 Approved.
| Available Properties |
- Viscosity
- Hardness, Shore D
- Surface Resistivity per Square
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Capillary Flow
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|