Loctite® 5071 Silicone Encapsulant
Subcategory: Silicone; Adhesive; Thermoset
Material Notes:
Conformal Coatings Conformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.
Loctite® 5071 Silicone Encapsulant A paste UV curable silicone coating that provides stress relief for thermal cycling. Permits easy removal for component repair. Cure Type: UV
| Available Properties |
- Viscosity
- Hardness, Shore A
- Surface Resistivity per Square
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|