Loctite® 3619 CHIPBONDER® Low Temperature Cure, Syringe Dispense

 

Subcategory: Adhesive; Thermoset

Material Notes:

Surface Mount Adhesives
Loctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application techniques including syringe dispense, stencil print and pin transfer.

Loctite® syringe dispense products provide unmatched performance for electronics assembly:

  • High Speed Dispense
  • Low Temperature Cure
  • Products for difficult-to-bond substrates


Loctite® 3619 CHIPBONDER® Low Temperature Cure, Syringe Dispense
A low temperature curing adhesive designed for high-speed syringe dispense.

Peaked dot profile.

Process Method:

  • High speed
  • Syringe dispensing
  • 40,000 DPH capable

Storage (Protect from heat): 40°F (+/-5°F) or 5°C (+/-3°C)

Available Properties
  • Cure Time
  • Shelf Life
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。