Loctite® 5248 Silicone Adhesive
Subcategory: Silicone; Adhesive; Thermoset
Material Notes:
Medical Grade Bonders Loctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designed specifically for the assembly of medical devices where toxicity testing and sterilization resistance are required.
Loctite® 5248 Silicone Adhesive A self-leveling UV silicone ideal for sealing and bonding extruded and moldable silicones, glass, and metals. Key Substrates: Elastomer, metal, glass Cure Type: Ultraviolet, Moisture
| Available Properties |
- Brookfield Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|