Loctite® M-06FL Durabond® Urethane Adhesive
Subcategory: Adhesive; Polyurethane, TS; Thermoset
Material Notes:
Medical Grade Bonders Loctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designed specifically for the assembly of medical devices where toxicity testing and sterilization resistance are required.
Loctite® M-06FL Durabond® Urethane Adhesive A urethane adhesive that forms highly flexible joints. An off-white, medium-viscosity urethane ideal for use on metals, plastics, glass and other substrates. Key Substrates: Thermoplastic, thermoset plastic, polycarbonate, elastomer, metal, glass, ceramic Cure Type: Room Temperature
| Available Properties |
- Brookfield Viscosity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|