Luvocom® 1105/GR/15/TF/15-2 Graphite and PTFE Filled PEEK
Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic; Polymer
Material Notes: Description: Luvocom® materials from this product group are not adversely affected by long operating periods at very high temperatures; PPA and PSU can cope with 160 °C, PPS will tolerate over 220 °C and PEEK or PAEK can be used at up to 260 °C. Other exceptional features include: nonburning properties (no addition of flame retarding agents required), low creep, high dimensional stability, sterilisability. Typical applications are for parts subjected to high stresses in car engines or other areas of mechanical engineering and in medical equipment. Processing: Luvocom can generally be processed on commercial injection molding machines, provided that the injection unit has been well designed and common technical rules have been obeyed. Barrels and plasticizing screws should be protected against wear as usual for processing reinforced thermoplastic compounds. Added fibers and fillers could act abrasive. It is urgently advised to pre-dry the pellets with an appropriate dryer just before processing. Information provided by Lehmann & Voss.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Coefficient of Friction, Static
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|