Luvocom® 50/CF/15/TF/15/SI/2/BK Silicone, Carbon Fiber and PTFE Filled Polycarbonate
Subcategory: Polycarbonate; Thermoplastic; Polymer
Material Notes: Description: Components which are subjected to severe dynamic forces need to have a low specific weight coupled with high mechanical strength and stiffness. Luvocom® high-performance materials provide exactly these qualities. Further benefits of this group of products are: a low coefficient of linear thermal expansion, greater thermal conductivity and excellent dimensional stability. A tensile strength of > 250 MPa is possible using Luvocom®, at a tensile modulus of > 30,000 MPa. Carbon fiber reinforced polymers are used in rapidly moving parts in machines and apparatuses, such as thread guides, pump slide valves, gear teeth, cams and connecting rods. Carbon fiber reinforced materials have also proved to be a viable alternative to aluminum for the manufacture of casings. Processing: Luvocom can generally be processed on commercial injection molding machines, provided that the injection unit has been well designed and common technical rules have been obeyed. Barrels and plasticizing screws should be protected against wear as usual for processing reinforced thermoplastic compounds. Added fibers and fillers could act abrasive. It is urgently advised to pre-dry the pellets with an appropriate dryer just before processing. Information provided by Lehmann & Voss.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Coefficient of Friction
- Coefficient of Friction, Static
- Limiting Pressure Velocity
- Surface Resistance
- Insulation Resistance
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Vicat Softening Point
- Processing Temperature
- Nozzle Temperature
- Zone 1
- Zone 2
- Zone 3
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|