Master Bond One Component Epoxy EP3HT
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Rapid curing, heat resistant, general purpose adhesive/sealant. Superior physical and electrical properties. Ideal for manufacturing applications. Bonds well to a broad range of substrates.Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Storage Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
|
|
|
|