Master Bond One Component Epoxy EP3RR-1
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Toughened system featuring rapid curing, good thermal conductivity & heat resistance. Excellent flowability. Primarily for potting & underfill applications. Castable over 1 inch thick.Information provided by Master Bond Inc.
| Available Properties |
- Viscosity
- Storage Temperature
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
|
|
|
|