Master Bond One Component Epoxy EP36AO
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Thermally conductive version of EP36. Semi-flexible. For potting and encapsulation. Good heat transfer properties. Suitable for moderate size castings. Good mechanical and thermal shock
resistance. Passes Class H thermal insulation tests.Information provided by Master Bond Inc.